Fatigue Crack Growth Mechanisms for Nickel-based Superalloy Haynes 282 at 550-750 °C
Fatigue Crack Growth Mechanisms for Nickel-based Superalloy Haynes 282 at 550-750 °C
,
Rozman, K. A.
,
Kruzic J. J.
,
Sears J. S.
, and
Hawk J. A.
, Journal of Materials Engineering and Performance, Volume 24, Issue 10, p.3699-3707, (2015)